Hard high temperature foundry quality refractory bricks. Dimensionally half the thickness of standard refractory bricks. Used for blacksmith forge and foundry floors, wall and hearths.

1.25 x 4.5 x 9 inches (32 x 114 x 229mm)

3.75 lb.(1.701 kg)

Box of 5 bricks includes USPS Flat Rate Priority Mail shipping.
Stack of split fire bricks

Details

Hard high temperature foundry quality refractory bricks. Dimensionally half the thickness of standard refractory bricks

1.25 x 4.5 x 9 inches (32 x 114 x 229mm)

3.75 lb.(1.701 kg)