Morgan Thermal Ceramics ceramic blanket insulation. Kaowool Cerablanket and NEW Superwool low biopersistence fiber insulation. We sell cut lengths from 1 foot to full rolls and on pallets in truckload quantities.  6 and 8 pound density blanket in 1/2" (13 mm), 1" (25mm) and 2" (50mm) thicknesses. 

NOTE: The higher rated Cerablanket has replaced Kaowool RT.  As inventories are sold out there will no longer be material packaged as RT. 

Kaowool Cerablanket 2,400°F
1,315°C
High purity refractory blanket with high temperature rating.
We sell Cerablanket HP in cut lengths as well as full cartons up to truck load quantities. Inventoried in our shop and warehouse.
Superwool® 2,372 F
1,300°C
New low biopersistence Alkaline Earth Silicate refractory blanket. Superwool® Fibre meets the requirements requested under NOTA Q. If you are looking for an environmentaly friendly, healthy alternative to standard refractory fibres, this is the one.  NOT recommended for forges or buner chamber lining.
Kaowool RT 2,300°F
1,260°C
Previously the "standard" refractory blanket for most applications. Has beeen replaced by Cerablanket. Generally no longer available.

Uniform carton size: 25 x 19 x 19" (63.5 x 48.3 x 48.3cm) - 4.16 cu.ft. (0.118 m3) rolled material.

Kaowool Cerablanket Cut Lengths

Kaowool is the original asbestos replacement material invented by Babcock and Wilcox. Cerablanket ( Cera Wool) - 2,400°F / 1,315°C, 6 PCF (Pounds per Cubic Foot) density material in 1/2 inch through 2 inch blanket. We sell cut lengths and full cartons.  NOTE: Kaowool Cerablanket is replacing Kaowool RT at the same price.


...See Detail
Kaowool Cerablanket HP Full Cartons

Cerablanket ( Cera Wool) - 2,400°F / 1,315°C, 6 and 8 PCF blanket in 1/2 inch through 2 inch in full cartons.  Quantity discounts apply over 6 cartons. Kaowool is the original high temperature asbestos replacement material invented by Babcock and Wilcox and now a trademark product of Morgan Thermal Ceramics.


...See Detail
Superwool 607 HT
Superwool 607 HT low biopersistence ceramic insulation blanket with the highest temperature rating of an Alkaline Earth Silicate Wool blanket.
...See Detail
Superwool 607 HT Full Cartons
Superwool 607 HT low biopersistence ceramic insulation blanket with the highest temperature rating of an Alkaline Earth Silicate Wool blanket.