Quick Overview

A safe clean graphite free water soluble lubricant used for hot forging steel parts and blacksmith hand and press punching. This product can be used for most forging operations to reduce tool wear and improve forging quality. Undiluted concentrate packaged in small quantities for the blacksmith or small forge shop.
forge ease 3512 - 640

More Views

  • Fuchs Forge Ease 3512
  • back label with QR code 640
  • forge ease gallon 640

Details

Fuchs Forge Ease 3512 Punch Lube. A water soluble alkaline salt lubricant used for hot forging steel parts. This product can be used for most hot forging operations and is an exceptional punch lube.

  • Reduces wear and tear on tools.
  • Clean, no smoke, no dirty black residue
  • Improves forging quality
  • Environmentally Friendly

Undiluted concentrate packaged in small quantities for the blacksmith shop. We sell gallons, half gallons, quarts and pints in convenient plastic F-style handled jugs.

A forge lubricant should be used for all types of punching, hot or cold. For hot punching blacksmiths have used everything including beeswax, axle grease, coal dust, graphite with soap, Never Seize and other proprietary mixtures. Any of these is better than nothing but none perform like a commercially formulated alkaline salt lubricant.

Hot punching with Forge Ease 3512 takes less effort and reduces wear on tools. In industry. Forge Ease 3512 is diluted with water and sprayed onto dies between parts. In the blacksmith shop warm tools are dipped in diluted lube as they are used. Besides use on punches and hot cuts. Forge Ease 3512 can be used on any cavity die, clapper die or character punch to reduce wear and let the metal flow more easily. This improves detail on letter and hallmark or touch mark stamps.

Adobe PDF Document FUCHS Forge Ease Technical Data Factory information sheet.

Adobe PDF Document FUCHS Forge Ease 3521 SDS Material Safety Data Sheet.

FORGE EASE Review Testimonial/Review by Pete Johnson of Nomad Forge and Ironworks

FORGE Lube Testimonial from Jeff Reinhardt AKA Ptree of Persimmon Tree Forge

Blacksmith Punch Lube Comparison Test Report from Jeff Reinhardt AKA Ptree of Persimmon Tree Forge